0
Article Sign in to save

Multi-Regional Natural Aging Behaviors and Degradation Mechanisms of Polyurethane-Coated Fabrics Under Coupled Multiple Environmental Factors

AI summary Read the abstract

Researchers conducted 24-month natural aging tests on polyurethane-coated tarpaulin fabrics across three climatically distinct regions of China, finding that tropical conditions (high heat, humidity, and UV) caused the most severe degradation — reducing tear strength by over 50% — with hydrolysis and oxidation identified as the dominant breakdown mechanisms.

Polymers

Polyurethane-coated fabrics are widely employed as tarpaulin materials. However, due to the long duration and large space requirements of natural exposure tests, studies on fabric degradation remain scarce. To systematically investigate the natural aging patterns and mechanisms of polyurethane-coated fabrics, this study conducted 24-month natural aging tests in three representative regions: Xishuangbanna (tropical monsoon climate), Xiamen (subtropical maritime monsoon climate), and Jinan (temperate monsoon climate). Changes in appearance, mechanical properties, surface morphology, elemental composition, and microstructure were thoroughly analyzed. The results indicated that gloss decreased by over 60%, the color difference exceeded 5.8, and tear strength was reduced by more than 50%. SEM, ATR-FTIR, and XPS analyses revealed that hydrolysis and oxidation occurred in the coating, leading to coating thinning, fiber exposure, and even damage. In Xishuangbanna, high temperature, high humidity, and strong solar radiation are responsible for the most severe degradation of fabrics. High temperature, humidity, and salt fog synergistically accelerated the aging process. In Jinan, significant thermal strain contributed to deterioration, and fabrics exhibited the mildest degradation. This multi-region natural exposure study realistically simulates in-service aging behavior, providing important validation for accelerated laboratory aging methods, product reliability improvement, and service-life modeling.

More Papers Like This

Article Tier 2

Releases of microplastics and chemicals from nonwoven polyester fabric-based polyurethane synthetic leather by photoaging

AI summary Read the abstract

Researchers compared microplastic fiber release and chemical transformation from polyurethane-coated synthetic leather and uncoated nonwoven PET fabric under UV photoaging, finding that the PU coating reduced fiber release but increased the degree of chemical oxidation. Photoaging of synthetic leather products produces microplastic fibers and chemical breakdown products that enter aquatic environments.

Article Tier 2

An Outdoor Aging Study to Investigate the Release of Per- And Polyfluoroalkyl Substances (PFAS) from Functional Textiles

AI summary Read the abstract

Researchers investigated the release of per- and polyfluoroalkyl substances from functional textiles during outdoor weathering in Sydney, finding that PFAS-treated polyamide fabrics release fluorinated compounds into the environment through aging and degradation.

Article Tier 2

Insight into Degrading Effects of Two Fungi on Polyurethane Coating Failure in a Simulated Atmospheric Environment

AI summary Read the abstract

Researchers found that two fungi collected from an atmospheric corrosion site — Talaromyces funiculosus and Phanerochaete chrysosporium — caused measurable biodegradation of polyurethane coatings under high humidity conditions, revealing biological pathways for polymer coating failure.

Article Tier 2

Long-term localization experiments reveal aging degradation mechanisms of biobased and petroleum-based polyurethanes in natural environments: degradation characteristics, product assessment and degradation cycle prediction

AI summary Read the abstract

Researchers conducted a 807-day field localisation experiment to study the degradation mechanisms of biobased and petroleum-based polyurethanes used as polymer coatings on controlled-release fertilisers in natural soil environments. The study characterised the degradation products, assessed environmental risk, and developed a predictive model for the degradation cycle, finding that both polyurethane types fragment into microplastic residues at different rates.

Article Tier 2

Physicochemical and biological ageing processes of (micro)plastics in the environment: a multi-tiered study on polyethylene

AI summary Read the abstract

Researchers studied how polyethylene undergoes both physicochemical and biological aging simultaneously in natural environments, finding that combined aging processes differ from each individually studied in isolation. Exposure to UV light, moisture, and microorganisms altered the plastic's surface chemistry and fragmentation pattern in ways that standard single-factor tests missed. This multi-tiered approach better reflects how microplastics actually degrade in nature.