0
Article ? AI-assigned paper type based on the abstract. Classification may not be perfect — flag errors using the feedback button. Tier 2 ? Original research — experimental, observational, or case-control study. Direct primary evidence. Detection Methods Environmental Sources Human Health Effects Marine & Wildlife Sign in to save

Screening of polymer types and chemical weathering in macro- and meso-plastics found on lake and river beaches using a combined chemometric approach

Analytical Methods 2022 5 citations ? Citation count from OpenAlex, updated daily. May differ slightly from the publisher's own count. Score: 40 ? 0–100 AI score estimating relevance to the microplastics field. Papers below 30 are filtered from public browse.
Nicolas Nayrac, Jean‐Philippe Bellenger, Pedro A. Segura

Summary

Researchers developed a combined chemometric approach using ATR-FTIR and Raman spectroscopy to screen polymer types and assess UV-induced chemical weathering in macro- and meso-plastics collected from lake and river beaches, finding that oxidation and carbonyl group formation are key markers of environmental degradation.

Polymers
Study Type Environmental

In the environment, synthetic polymers, commonly known as "plastics", are well-known to undergo various chemical weathering processes, which modify their surface chemistry by introducing new functional groups. Such changes are important to monitor, as they can severely influence the toxicity caused by plastic debris. Therefore, in this study, two chemometric models are proposed to accelerate the chemical classification of macro- and meso-plastics found in the environment. For this purpose, principal component analysis (PCA) and hierarchical cluster analysis (HCA) were applied on preprocessed infrared spectra of 83 plastic fragments found on public lake and river beaches. HCA associated all beach samples with a known plastic, whereas PCA enabled the association of only 39.8% (33 out of 83) of the beach samples with a known plastic. However, both techniques agreed on 93.9% of the samples identified. According to PCA and HCA results, polypropylene and polyethylene were the most frequently identified polymers in the samples. PCA turned out to be a very promising tool for fast screening of weathered plastics, since the distance of samples from the polypropylene cluster in the PCA plot was correlated with weathering. This was later confirmed by employing other characterization techniques such as micro-Raman, X-ray photoelectron spectroscopy and scanning electron microscopy. Finally, future experiments should focus on the applicability of the proposed combined chemometric approach for very small microplastics (<100 μm), as they have more important effects than larger plastics on aquatic ecosystems.

Sign in to start a discussion.

More Papers Like This

Article Tier 2

Optimizing microplastic analysis through comparative FTIR and raman spectroscopy: Addressing challenges in environmental degradation studies

This study optimized microplastic analysis by comparing FTIR and Raman spectroscopy approaches for identifying degraded polymer particles in environmental samples where photooxidation and mechanical fragmentation have altered spectral signatures. A combined spectroscopy approach outperformed either technique alone for accurately identifying degraded microplastics in complex environmental matrices.

Article Tier 2

A New Chemometric Approach for Automatic Identification of Microplastics from Environmental Compartments Based on FT-IR Spectroscopy

Researchers developed a new chemometric approach for automatic identification of microplastics from environmental samples, designed to handle the challenges of biofilm contamination and surface aging that typically impede standard spectroscopic characterisation methods.

Article Tier 2

Challenges of Raman spectra to estimate carbonyl index of microplastics: A case study with environmental samples from sea surface

Researchers assessed the feasibility of using carbonyl index (CI) values from Raman spectra as an indicator of polyethylene microplastic degradation, comparing them to CI values from FTIR spectra on the same environmental seawater samples. Despite some correlations observed between the two methods, the weak functional relationships suggest Raman CI cannot reliably substitute for FTIR CI as a degradation indicator.

Article Tier 2

Handheld portable FTIR spectroscopy for the triage of micro and meso sized plastics in the marine environment incorporating an accelerated weathering study and an aging estimation

Researchers tested a handheld portable FTIR spectrometer for rapidly identifying micro and mesosized plastic debris on beaches and in the marine environment. Portable FTIR devices enable fast field identification of plastic polymer types, making marine litter surveys more efficient.

Article Tier 2

Characterizing photochemical ageing processes of microplastic materials using multivariate analysis of infrared spectra

Researchers tracked how four common plastic types weather under UV light and sunlight over six months, using infrared spectroscopy and multivariate analysis to characterize surface chemistry changes. They found that polypropylene weathered fastest, while all plastics showed photooxidation at different rates depending on light source. The study proposes a multivariate spectral approach as a more broadly applicable method than the traditional carbonyl index for assessing microplastic aging.

Share this paper