0
Article ? AI-assigned paper type based on the abstract. Classification may not be perfect — flag errors using the feedback button. Tier 2 ? Original research — experimental, observational, or case-control study. Direct primary evidence. Remediation Sign in to save

Carbon Fiber Reinforced Recycled Polypropylene/Polyolefin Elastomer Composites with High Mechanical Properties

Polymers 2024 5 citations ? Citation count from OpenAlex, updated daily. May differ slightly from the publisher's own count. Score: 45 ? 0–100 AI score estimating relevance to the microplastics field. Papers below 30 are filtered from public browse.
Jin Wei, Abdukeyum Abdurexit, Abdukeyum Abdurexit, Ruxangul Jamal, Tursun Abdiryim, Jiangan You, Jiangan You, Zhiwei Li, Jin Shang, Qian Cheng

Summary

Researchers produced carbon fiber reinforced recycled polypropylene and polyolefin elastomer composites with enhanced mechanical properties, evaluating tensile strength, impact resistance, and fiber-matrix adhesion. Incorporating polyolefin elastomer improved toughness without substantially sacrificing stiffness, demonstrating a viable route to high-performance composites from recycled thermoplastics.

Polymers

The treatment of waste plastics has gradually become a hot topic in the current scientific community. In response to the needs for high-impact performance R-PP-based composites, carbon fiber (CF)-reinforced polyolefin elastomer (POE)/recycled polypropylene (R-PP) composite (CF/POE/R-PP) was prepared by the mechanical blending method, and its mechanical and thermal properties were systematically studied. It was found that the CF could effectively improve the bending and notch impact strength as well as enhance the thermal stability of POE/R-PP. Furthermore, a stable and dispersed composite interface formed by the combination of maleic anhydride-grafted polypropylene (PP-g-MAH) with the surface of CF and the fusion alkyl chains in R-PP and POE further enhanced the CF's reinforcing effect. As a result, the addition of 9 wt.% CF successfully improved the heat resistance of the composite material, and the residual carbon content increased by 97.84% after sintering. The composite toughening of POE and CF effectively improved the impact strength of the composite material, with a maximum increase of over 1000%. This study ultimately resulted in a high-impact-resistant composite material.