Design, Fabrication, and Properties of High Damping Metal Matrix Composites—A Review

Materials 2009 124 citations ? Citation count from OpenAlex, updated daily. May differ slightly from the publisher's own count. Score: 35 ? 0–100 AI score estimating relevance to the microplastics field. Papers below 30 are filtered from public browse.
Hui Lü, Xianping Wang, Tao Zhang, Zhijun Cheng, Q.F. Fang

Summary

This review covers the design and properties of metal matrix composites engineered for high vibration damping capacity, examining how to balance damping ability with mechanical strength. This materials engineering study has no connection to microplastics or environmental health.

Nowadays it is commonly considered that high damping materials which have both the good mechanical properties as structural materials and the high damping capacity for vibration damping are the most direct vibration damping solution. In metals and alloys however, exhibiting simultaneously high damping capacity and good mechanical properties has been noted to be normally incompatible because the microscopic mechanisms responsible for internal friction (namely damping capacity) are dependent upon the parameters that control mechanical strength. To achieve a compromise, one of the most important methods is to develop two-phase composites, in which each phase plays a specific role: damping or mechanical strength. In this review, we have summarized the development of the design concept of high damping composite materials and the investigation of their fabrication and properties, including mechanical and damping properties, and suggested a new design concept of high damping composite materials where the hard ceramic additives exhibit high damping capacity at room temperature owing to the stress-induced reorientation of high density point defects in the ceramic phases and the high damping capacity of the composite comes mainly from the ceramic phases.