Influence of Sample Wetting Method on ESC-Behavior of PMMA under Dynamic Fatigue Crack Propagation

Materials 2022 7 citations

AI summary Read the abstract

This study examined how environmental stress cracking in PMMA (acrylic glass) is accelerated under dynamic fatigue loading when the sample surface is wetted with a solvent. Different wetting methods produced different degrees of crack propagation acceleration. The results are relevant to understanding how plastic components degrade in outdoor environments where they are exposed to both mechanical stress and chemical exposure.

Polymers

Environmental stress cracking (ESC) is one of the most prominent failure mechanisms for polymer components. The high sensitivity of plastics in regard to environmental influences has always meant that plastics as materials have been viewed very critically in outdoor applications. Recently, the massive occurrence of microplastics in the environment means that questions about the long-term stability of plastic parts and the studies of plastic fragmentation are of great scientific interest. ESC behavior also plays an important role in connection with the formation of microplastics. In this work, the influence of two different sample wetting methods on ESC behavior was investigated. In case A, the sample was in situ wetted with the medium during the measurement by using a sponge. In case B, the sample was wetted by storage in the medium prior to measurement. Different stress cracking agents (SCA) were examined for polymethylmethacrylate (PMMA). Fracture-mechanical fatigue crack propagation (FCP) tests were carried out to quantitatively determine the sensitivity to ESC. Correlations between the absorption behavior and the ESC behavior of the SCA and the resulting morphological phenomena were established. Depending on the wetting method, significant differences in FCP were observed. The in situ wetting of the samples (case A) during the FCP measurement with ethylene glycol (EG) and with deionized water (DI) led to a significant shift in the crack propagation curves to higher ∆K—compared to the PMMA reference. In the case of n-heptane (NH), a more brittle crack propagation behavior was observed due to the chemical interaction with PMMA. The previously immersed samples (case B) give different results. Storage in NH and EG showed no influence on the crack propagation behavior. Samples immersed in DI showed a completely different course of crack growth. At a certain load, a sudden deceleration of the crack propagation and thus a horizontal curve could be seen. Above a certain ∆K value, crack growth began again. Depending on the immersion time (14, 30, or 60 days), this so-called stepped behavior shifted to lower da/dN values.

More Papers Like This

Article Tier 2

Wettability after Artificial and Natural Weathering of Polyethylene Terephthalate

AI summary Read the abstract

Researchers systematically studied how artificial and natural weathering of polyethylene terephthalate (PET) changes its surface wettability, finding that contact angle measurements combined with FTIR analysis can reliably track the progression of plastic degradation in aquatic environments.

Article Tier 2

Combined effect of artificial aging and fatigue on the mechanical, structural, and morphological properties of polystyrene

AI summary Read the abstract

This study found that combining UV-B exposure with mechanical fatigue significantly accelerated the degradation of polystyrene, reducing molecular weight and mechanical strength beyond what either stressor caused alone. This combined weathering process accelerates microplastic formation from polystyrene products in outdoor environments.

Article Tier 2

Effects of Weathering on Microplastic Dispersibility and Pollutant Uptake Capacity

AI summary Read the abstract

This study examined how environmental weathering changes the surface properties of microplastics and their ability to absorb co-pollutants, finding that weathered MPs bind more contaminants than pristine particles due to surface oxidation and cracking. The results emphasize that the environmental fate and toxicity of microplastics change dynamically as they age in the environment.

Article Tier 2

Study of the Effect of Accelerated Aging by Sea Water on the Mechanical and Chemical Properties of High Density Polyethylene Bottles

AI summary Read the abstract

Researchers subjected high-density polyethylene bottle samples to accelerated seawater aging at two temperatures, finding that immersion caused a loss of ductility and a transition from ductile to brittle failure behavior, with FTIR analysis confirming increasing crystallinity and SEM revealing progressive surface degradation over the aging period.